N2XOH 0,6/1 kV 3-1x300 mm2

Description

Description

Application:

In low voltage power distribution networks. Special application in places with poor ventilation, direct application in places with public attendance high. It can be installed in ducts, ladders or cable trays, in dry, humid or wet environments.

Construction:

1. Conductor: Soft copper, class 2.

2. Insulation: Cross linked polyethylene XLPE.

3. Outer sheath: Halogen free thermoplastic compound HFFR-UV.

4. Tape: Polyester tape.

Main characteristics:

The cable has excellent electric properties. The cross-linked polyethylene insulation allows a higher power capacity current under any operation conditions, lower dielectric losses, high insulation resistance. The outer sheath has the following characteristics: Fire retardant, zero emission dense smoke and halogen free. Sunlight resistance.

Cross section:

From 6 mm2 up to 500 mm2.

Marking:

INDECO S.A. N2XOH 0,6/1 kV (3 or 2) - 1 x Section - Year (- sequential length m. || sequential length m. + ).

Packing:

Non returnable wooden reels.

Colour:

Insulation: Natural.

Outer sheath: White, black, and red, or blue, black and red or white and black.

National standards

NTP-IEC 60228: Conductors of insulated cables.

NTP-IEC 60502-1: Power cables with extruded insulation and their accesories for rated voltages of 1 kV and 3 kV.

International standards

IEC 60228: Conductors of insulated cables.

IEC 60502-1: Power cables with extruded insulation and their accesories for rated voltages of 1 kV and 3 kV.

IEC 60332-1-2: Test for vertical flame propagation for a single insulated wire or cable - Procedure for 1 kW pre-mixed flame.

UL 2556: Wire and Cable Test Methods. Section 9.3: FT1 (Vertical-Specimen) Flame Test.

IEC 60332-3-24: Test for vertical flame spread of vertically-mounted bunched wires or cables - Category C.

IEC 60754-1: Test on gases evolved during combustion of materials from cables - Part 1: Determination of the halogen acid gas content.

IEC 60754-2: Determination of degree of acidity of gases evolved during the combustion of materials taken from electric cables by measuring pH and conductivity.

IEC 61034-2: Measurement of smoke density of cables burning under defined conditions.

ICEA S-95-658: Power cables rated 2000 volts or less for the distribution of electrical energy. Section 6.4.2: Oil Immersion Test.

UL 2556:Wire and Cable Test Methods. Section 4.2.8.5: Carbon-Arc and Xenon-Arc Tests- Sunlight resistance.

Calculation of Current Condition: Copper Conductor Triple L.V.; 90°C

CURRENT CAPACITY VALUES AND CURRENT CALCULATION CONDITIONS BASED ON IEC 60364-5-52:2009 :

TABLE B.52.5 (METHOD D1: Buried duct in contact).
TABLE B.52.5 (METHOD D2: Buried in contact).
TABLE B.52.12 (METHOD F: Air in flat formation and in contact).
TABLE B.52.12 (METHOD F: Air in triangular formation).

Maximum conductor temperature : 90°C.
Ambient air temperature : 30°C.
Ground temperature : 20°C.
Depth of laying up to: 0,7 m.
Thermal resistivity of soil : 2,5 K.m/W.

Characteristics

Characteristics

Construction characteristics

Construction characteristics

Conductor material
Soft copper
Insulating material
XLPE
Individual sheath
Halogen free thermoplastic compound - UV
Halogen free
Low content Halogen IEC 60754-1
Conductor flexibility
Class 2 IEC 60228
Conductor shape
Compact stranded
Insulation
XLPE
Sheath colour
Individual Sheath Red-Black-Blue
With Green/Yellow core
No

Dimensional characteristics

Dimensional characteristics

Number of cores
3
Conductor cross-section
300 mm²
Conductor diameter
20.2 mm
Total number of wires
37
Minimum insulation thickness
1.8 mm
Minimum outer sheath thickness
1.2 mm
Height
26.7 mm
Width
79.7 mm
Approximate weight
8702 kg/km

Electrical characteristics

Electrical characteristics

Rated Voltage Uo/U (Um)
0.6/ 1 (1.2) kV
Dielectric strength
3.5 kV
Max. DC resistance of the conductor at 20°C
0.0601 Ohm/km
Time of application Dielectric strength core to screen AC
5 min.
Nominal capacitance
802.0 pF/m
Perm. current rating in air 30°C - flat formation
736 A
Perm. current rating in air 30°C - trefoil formation
703 A
Permissible current rating buried 20°C
419 A
Permissible current rating buried/duct 20°C
365 A

Usage characteristics

Usage characteristics

Oil resistance
ICEA S-95-658
Gases toxicity
Zero toxicity to IEC 60684-2
Gases corrosivity
Low Corrosivity IEC 60754-2
Smoke density
Low Smoke Emission IEC 61034-2
Flame retardant
IEC 60332-1-2; FT1
Fire retardant
EN IEC 60332-3-24 (cat C)
Metric marking
-
U.V resistance
UL 2556 - Sunlight Resistance
Maximum operating temperature
90 °C
Overload maximum core temperature
130 °C
Short-circuit max. conductor temperature
250 °C
Midspan
No

Resources

Resources

Dealer locator

Waiting…

No items found

Contact us

Topics on which you wish to get more informations:

Required fields*

Please check your entry and try again.

An email address must contain a single @

Personal data protector

You have the right to object to the processing of your personal data and/or their use for direct marketing or commercial purposes

Thank you!

Thanks for contacting us. We will be in touch with you shortly.

Error

An error occurred. Please try again.

Close

Contact us

Required fields*

Please check your entry and try again.

An email address must contain a single @

Personal data protector

You have the right to object to the processing of your personal data and/or their use for direct marketing or commercial purposes

Thank you!

Thanks for contacting us. We will be in touch with you shortly.

Error

An error occurred. Please try again.

Close